Crystal Structure and Thermoelectric Properties of the Composite Crystal[(Ca1-xSrx)2CoO3]ρCoO2
Yuzuru MiyazakiTatsuro MiuraYasuhiro OnoTsuyoshi Kajitani
Author information
JOURNAL OPEN ACCESS

2003 Volume 50 Issue 6 Pages 475-479

Details
Abstract
Polycrystalline samples of [(Ca1-xSrx)2CoO3]ρCoO2 with 0≤x≤0.20 have been synthesized at 1193 K in flowing oxygen gas. The modulated crystal structure of the samples has been determined in accordance with a four-dimensional formalism from powder neutron diffraction data. With increasing x, the modulation amplitudes in Co-Co conduction paths become less marked. The non-doped sample (x=0) exhibits the resistivity ρ=150μΩm and the thermoelectric power S=130, μV/K at 300 K. Both the ρ and S values decrease with x but the decrease in ρ values is steeper than that of the S values. The power factor S2/ρ increases with x, from 110μW/m/K2 (x=0) to 140μW/m/K2 (x=0.20) at 300 K. This improvement in thermoelectric performance can be explained in terms of the reduction of displacive modulation of the Co-Co conduction paths in the CoO2 sheets.
Content from these authors
© Japan Society of Powder and Powder Metallurgy

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.
https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja
Previous article Next article
feedback
Top