Anisotropic Spring-back and Dimensional Change by Sintering of Iron Powder Compact
Hidenori Kuroki
Author information
JOURNAL OPEN ACCESS

1980 Volume 27 Issue 7 Pages 213-218

Details
Abstract
Radial and axial spring-backs of electrolytic iron powder compacts (φ10 ×h 10 mm) were determined. After the dewaxing at 600°Cfor 30 min and the sintering at 1100°C for 60 min in cracked-ammonia, the dimensional change of the compacts were measured.
The spring-back of the compacts containing zinc stearate increased with the pressure in both directions. The axial spring-back increased with the content of zinc stearate.
The dimensional change in the axial direction by sintering was a shrinkage which appeared to com-pensate a part of the porosity formed by the spring-back. While it was a dilation in the radial direction.
In the axial direction, there exists an obvious relationship between the spring-back and the dimensional change by sintering. But not in the radial direction
Content from these authors
© Japan Society of Powder and Powder Metallurgy

本論文はCC BY-NC-NDライセンスによって許諾されています.ライセンスの内容を知りたい方は,https://creativecommons.org/licenses/by-nc-nd/4.0/deed.jaでご確認ください.
https://creativecommons.org/licenses/by-nc-nd/4.0/deed.ja
Next article
feedback
Top